1. Longevity and doing of color coating systems are dependent on permissible building of the court. Consult the Asba (American Sports Builders Association) website for detailed guidelines.
Proper slope requirements are.8333% - 1.0%
Adequate face and subsurface drainage should be installed to prevent water accumulation beneath the surface.
Concrete courts should have a vapor barricade installed beneath the slab (10 mil thickness recommended).
Concrete Courts should be fulfilled, with a medium-broom texture, and no curing compounds should be used.
Consult the coating manufacturer's specifications and guidelines for full concrete making ready instructions.
2. Make sure that new asphalt or concrete is fully cured
28 days for concrete
30 days recommended for asphalt (during prime curing conditions of moderate sun to draw out oils and rain to rinse away.
Make sure that the existing face is not coated with a pavement sealer. Acrylics do not bond well to coal tar or most asphalt-based sealants.
Akdy Shower
3. face Repair
1 Hour after a rain or flooding the court, outline any puddle areas with chalk that cover a 5-cent piece (American coin). These areas should be repaired with Acrylic Patch Binder patching mix.
Fill all cracks over 1/8" wide with a favorable acrylic-based crack sealant. Never use a hot or cold applied asphalt-based crack filler.
4. Clean the court face prior to application of mend products or coatings. Any areas where mold, mildew, or fungus is clear should be treated with a clarification of 2 parts water to 1 part household bleach. Spray and broom in the bleach clarification and allow it to sit for 20 to 30 minutes. Scrub with brooms or favorable equipment, then rinse completely with a pressure washer. It's a good idea to treat any areas exposed to shade with this method.
5. All the time corollary the manufacturer's mixing instructions. Never over-dilute the coatings in order to "stretch" coverage. The specified sand size and shape are very important to the look and doing (speed of play) of the surface. If the permissible sand types are not ready in your area, purchase the coatings directly from the builder with sand pre-added.
6. corollary the manufacturer's application and curing temperatures
Apply products when temperatures are 50 degrees and rising
The best time to apply is in the morning when the face is cooler. If application during hot temperatures is unavoidable, the face can be lightly misted to cool the pavement. Do not puddle. Use a orchad pump sprayer or a hose nozzle with mist setting.
Acrylic Resurfacer and Color Coatings ordinarily dry within 1 hour of application in the full sun (based on 75 day with low humidity). Shade, low temperatures, and high humidity can increase drying times.
7. Use the permissible tools and equipment for mixing and application:
Floor Scrapers: Use to scrape foreign objects off of the face prior to application, and moderately scrape the face between coats to remove small bumps and imperfections. Do not scrape the discontinue coat.
Grass Trimmers: Trim around the court to prevent grass and weeds from hanging into the application path.
Blowers & Brooms: Blow, broom, and moderately scrape between coats.
Pressure Washer: Use to put in order face for color coating system. Blast the dirt and debris out of cracks and face voids.
Sport Squeegee: Make sure to use a squeegee that is designed for sport surfacing to minimize squeegee marks on the surface. A rubber blade that is 50 to 60 durometer (measure of softness) with a tapered/rounded edge is ideal.
Drill and Paddle Mixer: A 1 to 1.5 horsepower drill is recommended. Agitated tank systems are also available.
Line Taping Machine
8. permissible Application Technique
Watch an application video or consult a sport face builder for permissible application techniques
Have sufficient materials mixed for the entire coat before starting application.
Never squeegee the entire windrow dry during application, and make sure to pour the material directly into the existing wet puddle to minimize pour marks on the surface.
When applying the material by squeegee, only pull about ¼ of the entire width of the squeegee head. Pulling too much material at once can make it difficult to apply the coatings to the desired thickness.
Avoid putting the wet squeegee blade down on a dry, hot surface. Many times the squeegee blade lines can be seen straight through the discontinue coats. This is the same for wet shoes during application, so try to avoid stepping in the coating windrow.
9. All the time use a good quality masking tape for line striping, along with a line primer. This will minimize bleed under of the line paint for sharp lines. Two-inch wide masking tape is recommended for tennis court striping. One-inch tape works best for circles and arcs. The narrower tape can curve great without billowing.
10. 100% acrylic sport surfaces require very petite maintenance. However, normal cleaning will go a long way to extending the life of the surface.
Clean the court regularly: Once a month is suggested. Watch for evidence of mold or mildew in shaded areas and corners where organic debris tends to accumulate. Indoor courts require both frequent vacuuming and at least one every year wet vacuuming with mild detergent clarification and soft bristled equipment.
Remove Standing Water: Rain showers help clean your court. However, dirt accumulates in standing water, leaving stains. remove water from birdbaths as often as possible. Irrigation systems around the court should not spray on the court.
Remove foreign matter: Leaves and pine needles not only can stain your court, but also are breeding grounds for mold and mildew. It is especially important to remove leaves in the fall and keep your court free of debris all winter.
Use permissible equipment: Use soft nylon or hair-type brooms for scrubbing your surface. Scrubbing too hard with hard bristles can damage the surface. When using a water broom, limit pressure to 70 p.s.i. Be very true when using a power washer.